Manufacturing Process - Roll mylar film Alt
Description
Mylar film that can be coated with evaporated aluminum on one side
Characteristics
| Attribute | Value |
|---|---|
| Skill Level: | 2 |
| Tech Level: | 2 |
| Process Time: | 40.0 millisols |
| Work Level: | 10.0 millisols |
| Power Required: | 0.05 kW/hr |
Inputs
| Input | Amount |
|---|---|
| Polyester Resin | Resource |
| Polypropylene | Resource |
Products
| Produce | Amount |
|---|---|
| Mylar | 2.0 kg |
Version: pre-3.9.0 Generated on: 2024-12-28T22:56:23.2942481