Manufacturing Process - Purify rock salt into compounds

Description

http://www.madehow.com/Volume-2/Salt.html
			One method of evaporating brine is solar evaporation. Most brine is processed by a multiple-effect vacuum evaporator. This device consists of three or more closed metal cylinders with conical bottoms. Brine is first treated chemically to remove calcium and magnesium compounds. It then fills the bottom. Brine may also be processed in a grainer.

Characteristics

AttributeValue
Skill Level:1
Tech Level:1
Process Time:10.0 millisols
Work Level:10.0 millisols
Power Required:0.4 kW/hr

Inputs

InputAmount
rock saltResource

Products

ProduceAmount
calcium0.5 kg
calcium carbonate1.0 kg
calcium sulfate0.5 kg
epsom salt0.5 kg
magnesium0.5 kg
perchlorate1.5 kg
potassium0.5 kg
sodium carbonate1.0 kg
table salt1.5 kg

Version: pre-3.9.0 Generated on: 2024-12-28T22:56:23.2942481